¡Envío GRATIS por compras de S/89 o más!  Ver más

menú

0
  • argentina
  • chile
  • colombia
  • españa
  • méxico
  • perú
  • estados unidos
  • internacional
portada Perception of weld defects in digital X radiography images (en Inglés)
Formato
Libro Físico
Idioma
Inglés
N° páginas
128
Encuadernación
Tapa Blanda
Dimensiones
22.9 x 15.2 x 0.9 cm
Peso
0.18 kg.
ISBN13
9783311791706

Perception of weld defects in digital X radiography images (en Inglés)

Muthukumaran M (Autor) · Independent Author · Tapa Blanda

Perception of weld defects in digital X radiography images (en Inglés) - M, Muthukumaran

Libro Nuevo

S/ 144,75

S/ 289,50

Ahorras: S/ 144,75

50% descuento
  • Estado: Nuevo
Origen: Estados Unidos (Costos de importación incluídos en el precio)
Se enviará desde nuestra bodega entre el Lunes 05 de Agosto y el Lunes 19 de Agosto.
Lo recibirás en cualquier lugar de Perú entre 2 y 5 días hábiles luego del envío.

Reseña del libro "Perception of weld defects in digital X radiography images (en Inglés)"

X-radiography inspection techniques are generally used in non-destructive evaluationindustry. Manual assessment of the inspection may fail and turn into false assessment dueto a large number of examining while inspection process. Accordingly, incorrectassessment through human vision may cause immense industry disaster. Therefore, it isessential to examine through machine vision, which is capable to avoid false assessment.Digital X-radiography has widely been used in Non-Destructive Testing (NDT) andparticularly in weld defect detection. Weld defects occurrence is an unavoidable problemduring the welding process. Most common weld defects some of which are porosity, gaspore, tungsten inclusion, longitudinal crack, lack of penetration, and slag inclusion.Digital image processing techniques are a foremost way to experiment in the NDT. Thedetection and classification of weld defects depend on the quality of the digitized image, which is subjected to certain factors, such as noise, the mode of the image histogram, defects of different dimensions, indiscernible defects in the image background, and lowcontrast or unevenly illuminated image. More accuracy can be achieved during classificationof weld defects are always be subject to the deliverables of low and mid-level imageprocessing techniques. Therefore, it is desirable to provide more importance for these levelsin the weld X-radiography image.

Opiniones del libro

Ver más opiniones de clientes
  • 0% (0)
  • 0% (0)
  • 0% (0)
  • 0% (0)
  • 0% (0)

Preguntas frecuentes sobre el libro

Todos los libros de nuestro catálogo son Originales.
El libro está escrito en Inglés.
La encuadernación de esta edición es Tapa Blanda.

Preguntas y respuestas sobre el libro

¿Tienes una pregunta sobre el libro? Inicia sesión para poder agregar tu propia pregunta.

Opiniones sobre Buscalibre

Ver más opiniones de clientes